| Availability: | |
|---|---|
| Quantity: | |
| Hastelloy C-276(UNS N10276/W.Nr.2.4819/NS336) | ||||||||||||||
| Chemical Component | Alloy | % | Ni | Cr | Fe | Mo | C | Mn | Si | S | P | Co | V | W |
| C-276 | Min | Allowance | 14.5 | 4 | 15 | 3 | ||||||||
| Max | Allowance | 16.5 | 7 | 17 | 0.01 | 1 | 0.08 | 0.03 | 0.04 | 2.5 | 0.35 | 4.5 | ||
| Physical Property | Density | 8.89 g/cm3 | ||||||||||||
| Melting point | 1325-1370 ℃ | |||||||||||||
| The Minimum Mechanical Properties Of The Alloy At Room Temperature | Typical Mechanical Properties | Tensile Strength Rm N/mm2 | Yield Strength RP0.2N/mm2 | Elongation Rate A5 % | Brinell Hardness | |||||||||
| Solution Treatment | 690 | 283 | 40 | - | ||||||||||
| Hastelloy C-276(UNS N10276/W.Nr.2.4819/NS336) | ||||||||||||||
| Chemical Component | Alloy | % | Ni | Cr | Fe | Mo | C | Mn | Si | S | P | Co | V | W |
| C-276 | Min | Allowance | 14.5 | 4 | 15 | 3 | ||||||||
| Max | Allowance | 16.5 | 7 | 17 | 0.01 | 1 | 0.08 | 0.03 | 0.04 | 2.5 | 0.35 | 4.5 | ||
| Physical Property | Density | 8.89 g/cm3 | ||||||||||||
| Melting point | 1325-1370 ℃ | |||||||||||||
| The Minimum Mechanical Properties Of The Alloy At Room Temperature | Typical Mechanical Properties | Tensile Strength Rm N/mm2 | Yield Strength RP0.2N/mm2 | Elongation Rate A5 % | Brinell Hardness | |||||||||
| Solution Treatment | 690 | 283 | 40 | - | ||||||||||